日本財団 図書館


074-1.gif

Fig. 3.5 Compaction Curve for Galena

 

Transportable Moisture Limit (TML) determined through the test by Japan for each sample is given in Table 3. TML of Nickel Slag could not be determined because the degree of saturation did not reach 70 %.

 

Table 3 Transportable Moisture Limits determined by Proctor/Fagerberg Tests by Japan

074-2.gif

 

Similarly, TML determined through the test by Poland for each sample is given in Table 4.

 

Table 4 Transportable Moisture Limits determined by Proctor/Fagerberg Tests by Poland

074-3.gif

 

 

 